Description
SOLIBOND N
metal-to-ceramic Nickel-Chrome alloy
- beryllium free nickel-chrome alloy
- good manipulation when fluid, security is achieved by casting. Fast polishing, shining surfaces as well as burning stability of the alloy
- exact fitting and easy manipulation with a hardness of 180 HV
- very thin oxide layer, esthetic construction of the ceramic
- optimum metal-ceramic bonding
- durable, high corrosion resistance, can be scanned with laser
Tip: best casting results in combination with the investments YETIVEST, DUOVEST, YETI EXPANSION and YETI EXPANSION plus
Melting range | 1.250 – 1.330°C |
Casting temperature | 1390°C |
Vickers hardness | 180 HV |
Ultimate elongation | 25,0 % |
CTE (20 – 600°C) | 14,1 · 10-6 K-1 |
CTE (25 – 500°C) | 13,9 · 10-6 K-1 |
SOLIBOND N
Ni | Cr | Mo | Si | Fe |
62,7% | 24,5% | 10,4% | 1,4% | 1,0% |
Solibond N
1000 g | Art.-Nr. 963-1000 |